WebApr 27, 2012 · Polyimides, Water Abstract Depolymerization of polyimide synthesized from 4,4′-oxidiphthalic anhydride and 4,4′-diaminodiphenyl ether monomers (ODPA/ODA PI) … Webcurrent polyimide materials in terms of thermal stability and hydrolytic stability. Keywords: polymer, coatings, polyimide, fiber, wire, film 1 INTRODUCTION Polyimide polymers were discovered in the 1950’s through DuPont’s efforts to develop a processable polymer precursor that could be converted to a final polymer with very high
Low Dielectric Constant Polyimide Hybrid Films Prepared by in …
WebNIST Technical Series Publications WebMar 1, 2024 · These hydrolysis reactions are: (1) between OH − ions and the oxygen atoms covalently bonded to the pyromellitimide of polyimide and (2) between the positively … trailer backing techniques
Polyimide-Surface-Modified Silica Tubes: Preparation and …
WebDec 1, 2024 · Polyimide hydrolysis was conducted in stainless steel (SUS316) batch-type reactors with an internal volume of 6.8 cm 3. Before the experiment, each reactor was loaded with 3.4 g of 3.0 wt% hydrogen peroxide aqueous solution and heated at 673 … Recently, Wei et al. prepared polyimide nanocomposites with tethered … The reaction apparatus is shown in Fig. 1.The 90 cm 3 batch-type autoclave … Here, we focus the amount of gas except nitrogen in Table 1.The oxygen … Sub-critical water gasification by partial oxidation of glucose was carried out in … The hydrolysis rate increases exponentially with increasing temperature in aqueous … Fig. 3 shows the results for the series of reactions carried out above the critical … WebPolyimide films treated with an alkali and ion exchange undergo surface-confined hydrolysis to produce polyimide composites. On the other hand, it is unclear what impact this method has on the mechanical properties of PI films. This paper reports the effects of the mechanical properties of PI films exposed to an alkali (KOH) solution with different … WebFeb 24, 2024 · In order to elucidate more information about the chemical reactions undergone on the substrate, infrared spectroscopy has been used. Polyimide is insoluble in most solvents; hence, non-resinous polyimide liquid is usually supplied as a solution of polyamic acid (PAA) dissolved in NMP 27–31 When subjected to thermal imidization, i.e. … trailer ball attachment forklift